[email protected]

BAR (Cobalt Alloy 6B) - Magellan Metals

Hastelloy Nickel Alloys. Hastelloy C22® Hastelloy C276® Hastelloy B-2® Hastelloy X® Vascomax® Maraging Steel. Vascomax® 250 (Maraging 250 & C250) Vascomax® 300 (Maraging 300 & C300) Vascomax® C350 (Maraging 350 & C350) Haynes Metal Alloys. Haynes 25® Haynes 188® Rene 41® Multimet N155® Waspaloy® MP35N® MP159® Cobalt Alloy 6B Bearing Materials New Hampshire Ball Bearings, Inc.Cobalt Based ium Based Copper Based Aluminum Based Low Alloy Steels; BALL:303 440C PH13-8Mo 15-5PH 17-4PH A-286 BG42 ® Greek Ascoloy. Inconel ® 718 Inconel ® X-750 Rene 41 ® Waspaloy. Stellite ® 3 Stellite ® 6 Stellite ® 6B L-605 MP35N ® 6AI 4V. Al Bronze Al-Ni Bronze Beryllium Copper. 2024 6061 7075. 4140 4340 52100 M-2 M-42 M-50

CA2014694C - Corrosion- and wear-resistant cobalt-base

Disclosed is a cobalt-base alloy that has a valuable combination of both corrosion- and wear-resistant properties. The alloy nominally contains, in percent by weight, 25.5 chromium, 8.5 nickel, 3.0 iron, 5 molybdenum, 2 tungsten, 0.40 silicon, 0.75 manganese, 0.06 carbon, 0.08 nitrogen and the balance cobalt plus normal impurities normally found in alloys of this class. Cobalt Alloy product list - lookpolymersKennametal Stellite Tribaloy® T-401 Cobalt Alloy:Kennametal Stellite:Tribaloy® H.C. Starck Amperit® 415.6 CoNiCrAlY (MCrAlY) H.C. Starck:Amperit® Haynes 188 alloy, 30% cold reduction, 3.2 mm thick sheet, 1175°C for 5 minutes:Haynes International, Inc. Haynes 188 alloy, 40% cold reduction, 3.2 mm thick sheet, 1175°C for 5 Comparison of the sliding wear behaviour of self-mated Apr 30, 2019 · The cobalt-based alloys which are part of the Stellite family were first developed in the early 1900s and the main grades contain (in addition to cobalt) chromium, tungsten and carbon. The major difference between alloy grades is the carbon and tungsten levels, although control of minor elements such as Fe, Si, Mo, Ni, Mn and B is becoming

FIGHTS GALLING AND WEAR STRONGER THAN 304 /

cobalt-bearing and high nickel alloys. Its uniform corrosion resistance is better than Type 304 in most media. Chloride pitting resistance is superior to Type 316. Room temperature yield strength is nearly twice that of Types 304 and 316. In addition, NITRONIC 60 Stainless Steel provides excellent high-temperature oxidation resistance and HPAlloy listing sheetDistributor of cobalt alloys including L605, cobalt 6B & cobalt 6BH. Cobalt alloys are seizing, galling & wear resistance. Available in bar dia. ranging from 1/2 in. to 6 in. Cobalt 6B alloys are used for turbine engine nozzle fuel injectors, steam turbine, motor shafts, bushings, sleeves & stems. History of Haynes International, Inc.Haynes® alloy 6B, that has been in continuous production since its discovery. Patents were granted for other cobalt alloys as well. The business was incorporated in October, 1915 as Haynes Stellite Company. Over the course of the next year revenues for Stellite alloy exceeded $1,000,000. The company began to expand rapidly and had 20-25 employees in 1916.

KMT_Wear Solutions_Brochure - Kennametal - PDF Catalogs

There are more than 20 Stellite alloys in this family. A special Stellite alloy:Stellite 6B is a custom wrought (hot forged) material with outstanding resistance to most types of wear, and is extremely resistant to seizing or galling. High temperatures have little effect on the toughness and dimensional stability of this alloy. Nickel and Cobalt Alloys, Super Alloys, InconelAlloys International sources the best high-tech specialty metal mills throughout the world for your needs in nickel and other exotic & high temperature alloys, including hardfacing alloys such as Stellite. We provide the difficult alloys, sizes and specifications that others cant in nickel, cobalt, titanium and most other specialty alloys. Stellite Products & Suppliers Engineering360Description:Wear Resistant (Co-Cr-W) Cobalt 6B is a cobalt based chromium, tungsten alloy for wear environments where seizing, galling and abrasion are present. 6B is resistant to seizing and galling and with its low coefficient of friction, allows sliding contact with other metals without damage by metal pick

WEAR SOLUTIONS - Deloro

Stellite Alloys Stellite cobalt-based alloys are noted for their resistance to corrosion, erosion and abrasion at elevated temperatures (up to 800ºC). There are more than 20 Stellite alloys in this family. A special Stellite alloy:Stellite 6B is a wrought (hot forged) material with outstanding resistance to most Wear Resistant Alloys:NITRONIC and STELLITE for galling HPA Cobalt 6B (Co-Cr-W) (UNS R30016) Co 59.0, Cr 30.0, W 3.5, Ni 2.5, Mn 1.4, C 1.0 Excellent hot strength, which is fully returned when cooled to room temperature again. Replacement for castings due to better ductility, and dependability for sealing surfaces. stelite metal - casting-chinaSTELLITE® 20 ALLOY BALLS. Metal Alloys / Cobalt Based Alloys / Stellite® 20 Alloy Balls; STELLITE® 20 ALLOY BALLS. Co based alloy, usually STELLITE® trade name, that provide excellent wear resistance and high temperature resistance. Its microstructure is formed by a CoCr matrix and dispersed carbides. Balls are provided in the passivated

Cobalt Alloys - L605 - MP35N - Stellite 6B - Michlin Metals

Haynes 6B (aka Stellite 6B) UNS R30016 has a nominal composition of 58% Cobalt,2.5% Nickel, 30% Chromium, 4% Tungsten, 1.4% Mn, 3% Iron, and 1.5% Molybdenum.. A solid solution alloy for high temperature applications. MP-35N UNS R30035 is an alloy of 35% Cobalt, 35% Nickel,20% Chromium, and 10% Molybdenum.